Issue |
J. Phys. Colloques
Volume 48, Number C3, Septembre 1987
4th International Aluminium Lithium Conference
|
|
---|---|---|
Page(s) | C3-587 - C3-596 | |
DOI | https://doi.org/10.1051/jphyscol:1987368 |
4th International Aluminium Lithium Conference
J. Phys. Colloques 48 (1987) C3-587-C3-596
DOI: 10.1051/jphyscol:1987368
1 Ecole Centrale des Arts et Manufactures, F-92295 Châtenay-Malabry Cedex, France
2 CEA, B.P. 511, F-75752 Paris Cedex 15, France
J. Phys. Colloques 48 (1987) C3-587-C3-596
DOI: 10.1051/jphyscol:1987368
HYDROGEN EMBRITTLEMENT IN Al-Li-Cu-Mg ALLOYS (8090-T651)
F. BINSFELD1, M. HABASHI1, J. GALLAND1, J.P. FIDELLE2, D. MIANNAY2 et P. ROFIDAL21 Ecole Centrale des Arts et Manufactures, F-92295 Châtenay-Malabry Cedex, France
2 CEA, B.P. 511, F-75752 Paris Cedex 15, France
Abstract
This paper describes the hydrogen embrittlement (HE) of an Al-Li alloy aged at 190°C and with different durations of ageing (10, 15, 20 and 30 hr). Two techniques were employed to measure HE : a) cathodic polarization in a molten salts bath with -3 V/Ag on tensile specimens ; b) gaseous hydrogenation on disks. Hydrogen charging was achieved at 190°C. The results show that HE is important when the alloy is in the over-aged condition.