Numéro |
J. Phys. Colloques
Volume 48, Numéro C8, Décembre 1987
Fifth European Conference on Internal Friction and Ultrasonic Attenuation in Solids
|
|
---|---|---|
Page(s) | C8-95 - C8-100 | |
DOI | https://doi.org/10.1051/jphyscol:1987810 |
Fifth European Conference on Internal Friction and Ultrasonic Attenuation in Solids
J. Phys. Colloques 48 (1987) C8-95-C8-100
DOI: 10.1051/jphyscol:1987810
1 GEMPPM, Bât. 502, INSA, F-69621 Villeurbanne Cedex, France
2 Institut de Génie Atomique, Institut Fédéral Suisse de Techonologie, PHB-Ecublens, CH-1015 Lausanne, Switzerland
3 Dpto de Fisica del Estado Solido, Facultad de Ciencias, Aptdo 644, SP-48009 Bilbao, Spain
J. Phys. Colloques 48 (1987) C8-95-C8-100
DOI: 10.1051/jphyscol:1987810
MEDIUM TEMPERATURE PEAKS IN HIGH PURITY ALUMINIUM DOPED WITH 10 ppm COPPER OR SILVER
C. ESNOUF1, A. KULIK2, J.F. THEUMANN2 et M.L. NO31 GEMPPM, Bât. 502, INSA, F-69621 Villeurbanne Cedex, France
2 Institut de Génie Atomique, Institut Fédéral Suisse de Techonologie, PHB-Ecublens, CH-1015 Lausanne, Switzerland
3 Dpto de Fisica del Estado Solido, Facultad de Ciencias, Aptdo 644, SP-48009 Bilbao, Spain
Résumé
Les relaxations observées vers 0,5 Tm dans l'aluminium de
pureté ordinaire ont des caractéristiques assez différentes de celles observées
dans l'aluminium de très haute pureté. Dans cet article, les différences sont
analysées à partir d'échantillons de quatre puretés différentes.
Abstract
In the case of aluminium of ordinary purity, the observed
relaxations around 0,5 Tm have a behaviour which is different from that of high
purity aluminium. In this paper, the differences are analyzed using specimens
of four different purities.